Evaluation #2
SC Aircraft & Metal Cleaner Super Concentrate
20%
120°F
Yes
Heated Immersion at 120°F for 30 minutes with a stir bar for agitation, rinsed in a deionized water bath at 120°F for 30 seconds, dried with a heat gun